Szczeliwa grafitowe
Szczeliwo grafitowe ekspandowane
| P bar | V m/s | pH | temp. °C | |
|---|---|---|---|---|
| 20 | 25 | 1-14 | -200 ÷ +550 |
| 250 | – | 1-14 | -200 ÷ +550 |
| 180 | 2 | 1-14 | -200 ÷ +550 |
Szczeliwo grafitowe zbrojone inconelem
| P bar | V m/s | pH | temp. °C | |
|---|---|---|---|---|
| – | – | 1-14 | -200 ÷ +550 |
| – | – | 1-14 | -200 ÷ +550 |
| 250 | 2 | 1-14 | -200 ÷ +550 |
Szczeliwo grafitowe w oplocie ze stali inconelowej
| P bar | V m/s | pH | temp. °C | |
|---|---|---|---|---|
| – | – | 1-14 | -200 ÷ +600 |
| – | – | 1-14 | -200 ÷ +600 |
| 450 | 1 | 1-14 | -200 ÷ +600 |
Szczeliwo grafitowe z dyspersją PTFE
| P bar | V m/s | pH | temp. °C | |
|---|---|---|---|---|
| 20 | 20 | 1-14 | -200 ÷ +280 |
| – | – | 1-14 | -200 ÷ +280 |
| 100 | 2 | 1-14 | -200 ÷ +280 |